2010 FOAM SAMPLE
2010 FOAM SAMPLE
Specification
Article | D150/40 | D250/40 | D250/50 | D250/60 | D350/45 |
---|---|---|---|---|---|
Hardness (AskerC) |
35-45 | 35-45 | 45-55 | 55-60 | 45-50 |
Density (g/cm3) |
0.10-0.14 | 0.11-0.15 | 0.15-0.20 | 0.19-0.25 | 0.15-0.19 |
Article | D150/40 | D250/40 | D250/50 | D250/60 | D350/45 |
---|---|---|---|---|---|
Hardness (AskerC) |
35-45 | 35-45 | 45-55 | 55-60 | 45-50 |
Density (g/cm3) |
0.10-0.14 | 0.11-0.15 | 0.15-0.20 | 0.19-0.25 | 0.15-0.19 |